Journal of Yangtze River Scientific Research Institute ›› 2024, Vol. 41 ›› Issue (6): 164-170.DOI: 10.11988/ckyyb.20221695

• Hydraulic Structure and Material • Previous Articles     Next Articles

Rheology, Early Hydration Heat and Strength of Cement-based Materials Mixed with Steel Slag Powder and Silica Fume

MA Chao1,2,3, YAO Zhao-long1, YANG Zhao1,2,3, WANG Xin-long1, JIANG Dao-dong1,2,3   

  1. 1. CCCC Second Harbour Engineering Company Ltd.,Wuhan 430100,China;
    2. Research and Development Center of Transport Industry on Intelligent Manufacturing Technologies for Transport Infrastructure,Wuhan 430100,China;
    3. Key Laboratory of Transport Industry on Large-span Bridge Construction Technology, Wuhan 431400,China
  • Received:2022-12-20 Revised:2023-03-13 Online:2024-06-01 Published:2024-06-03

Abstract: To address the challenge of steel slag disposal, characterized by large quantities and low utilization rates, we prepared a green, low-carbon cement-based material with optimized mechanical properties by substituting part of the cement with steel slag ground into micro-powder and combined with silica fume. We conducted experimental studies on the rheological behavior, early hydration exotherm, strength, and water absorption of the prepared composite cement-based material system at various proportions. Our key findings are as follows: 1) Steel slag powder particles exhibits a less angular and flaky micro-morphology. When replacing 15% of the cement, steel slag powder effectively enhances matrix consistency, slightly reduces strength, and significantly decreases early hydration heat release by 8.8%, which is beneficial to the control of early temperature-induced cracking.2) Incorporating silica fume notably decreases the material’s plastic viscosity and pumping pressure. For applications requiring long-distance pumping, such as mass concrete or high-performance concrete, silica fume content should be limited to 5%. Additionally, silica fume’s space-filling effect and pozzolanic reaction enhances the material’s compactness and substantially improves strength. In summary, cement-based material incorporating 15% steel slag powder and 5% silica fume not only enhances pumping performance, strength, and durability but also mitigates early hydration heat release, demonstrating promising engineering applications.

Key words: steel slag powder, silica fume, rheology, early hydration heat, strength, water absorption